Breakpoints

Times are seconds from the start of the disturbance. Voltage is per-unit of nominal; frequency in hertz. An LVRT curve is a lower boundary (stay connected while voltage is on or above it), an HVRT curve an upper boundary, and FRT gives the band between its High and Low boundaries.

Event Duty Breakpoints Status
low-voltage ride-through (LVRT) ride-through 0.001s → 0 pu; 0.15s → 0 pu; 0.151s → 0.3 pu; 0.6s → 0.3 pu; 0.601s → 0.38 pu; 1.2s → 0.38 pu; 1.201s → 0.53 pu; 1.8s → 0.53 pu; 1.801s → 0.68 pu; 2.4s → 0.68 pu; 2.401s → 0.83 pu; 3s → 0.83 pu; 3.001s → 0.9 pu verified

Where these values come from

  • LVRT Philippine Grid Code, 2016 Edition (ERC Resolution No. 22, Series of 2016), GCR 4.4.4.4.1(a)-(d) and Figure 4.4 'Low voltage withstand capability – PVS'.